Ozokerafin Application Remedy Dr.Pirogov's Laboratory
- Characteristics
- Description
- How to use
- Ingredients
-
Age:
25+
Brand: Dr. Pirogov's Laboratory
Line: thermotherapy
Product Type: paraffin
Product Properties: repair, soothing, treatment
When To Use: universal
Gender: unisex
Classification: pharmacy
Country TM: Ukraine
Made in: Ukraine
The all-natural ozokeraphin product from the "Dr. Pyrogov Laboratory" brand is extracted from the Carpathian mountain rocks and is used for thermal therapy. This natural derivative of petroleum has a distinctive structure similar to paraffin. The therapeutic properties of this substance are characterized by a high saturation of hydrocarbons and a high melting point. When heated, ozokeraphin becomes warm and gently affects tissues and joints, soothes the nervous system, alleviates pain, and improves blood circulation.
The most common indication for using ozokeraphin applications is musculoskeletal disorders (such as arthritis, sciatica, and more), as well as post-injury rehabilitation. It is recommended to combine it with other treatment components, such as physiotherapy, therapeutic exercises, massage, electrophoresis, and mineral baths.
Contraindications: Ozokeraphin applications are contraindicated in cases of general contraindications to heat treatments, pregnancy, and sensitivity to the product's components.
-
There are three methods for applying the product:
- Layering: Melted ozokerite (at a temperature of 55-60°C) is applied to the skin using a brush.
- Napkin-Application: Fold gauze or bandage into 8-10 layers, immerse it in the melted ozokerite (at a temperature of 55-60°C), press out the excess, and apply it to the treatment area. Cover with a plastic wrap and then a blanket.
- Tray-Application: Pour the melted ozokerite into trays. Once it solidifies (at a temperature of 45-50°C), remove it from the tray along with the plastic wrap and apply it to the required areas.
Procedures should be conducted daily or every other day, lasting between 15 to 30 minutes per session. The course consists of 10-20 procedures. After each procedure, rest for 30-40 minutes.
-
Paraffin, ozokerite.